Induction hardening Jaw na hakoran Carbon Karfe

description

Babban yawan buguwa mai taurarawar Jaw Teeth na Carbon Karfe surface tsari

Manufa
Cikar hardening na haƙoran haƙoran ta amfani da shigowa.

Kayan aiki

DW-UHF-6KW-I na amfani da ingin harginging machine din

HLQ coil al'ada

Materials
Teethaƙƙarfan haƙoran ƙarfe wanda abokin ciniki ya kawo

Key Siffofin
Powerarfi: 4 kW
Zazzabi: Aƙalla 1526 ° F (830 ° C)
Lokaci: 10-15 sec

tsari:

  1. Anyi aikin coil na gwaji don aikace-aikacen.
  2. An gyara samfurin a wuri a ciki na murhun.
  3. An yi amfani da dumama dumin ciki a hakora.
  4. An kula da zazzabi na samfurin lokacin dumama.
  5. An yi amfani da zafi har sai an sami zafin jiki mai rauni.

results:

  • Tsarin gudanarwa don cimma iyakar ƙarfin sa.
  • An mai zafi zuwa 830 ° C a cikin 12 sec.
  • An kai 930 ° C a cikin 20 sec.
  • Matsayin Curie (kusan 770 ° C) an kai shi cikin 5 sec.

Ƙarshe:

  • Tsarin tsarin –DW-UHF-6KW-I ya dace da tsarin.
  • Classic coil kuma ya dace da wannan aikace-aikacen.

Shawara:

  • Za'a iya samun damar sarrafa kansa ta hanyar motsawa ko dai HS tare da coil ko muƙamuƙi a tsaye.
  • Dole ne a zabi tsarin sanyaya ingantacce. Ikon sanyaya sanyi - aƙalla 4kW. Za'a iya amfani da tsarin ruwa-iska, amma ya dogara da yanayin aikin yanayi.

 

=